Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VICTREX® PEEK 150GL30 BLACK - PEEK-GF30 - Victrex plc

Material Data Center offers the following functions for VICTREX® PEEK 150GL30 BLACK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Victrex PEEK datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.3 % ISO 294-4, 2577
Molding shrinkage, normal 0.9 % ISO 294-4, 2577
Thermal conductivity of melt 0.3 W/(m K) -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 12000 MPa ISO 527
Stress at break 190 MPa ISO 527
Strain at break 2.4 % ISO 527
Flexural modulus, 23°C 11500 MPa ISO 178
Flexural strength 270 MPa ISO 178
Izod impact strength, +23°C 50 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C 8.5 kJ/m² ISO 180/1A
Shore D hardness 87 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 343 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 143 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 335 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 20 E-6/K ISO 11359-1/-2
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 2 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Dissipation factor, 1MHz 40 E-4 IEC 62631-2-1
Volume resistivity 5E13 Ohm*m IEC 62631-3-1
Electric strength 21.5 kV/mm IEC 60243-1
Comparative tracking index 150 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.3 % Sim. to ISO 62
Density 1520 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 - 150 °C -
Pre-drying - Time 3 - 5 h -
Processing humidity ≤0.02 % -
Mold temperature 170 - 200 °C -
Feed temperature ≤100 °C -
Zone 1 360 °C -
Zone 2 365 °C -
Zone 3 370 °C -
Zone 4 375 °C -
Nozzle temperature 380 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Black
Special Characteristics
Sterilizable
Chemical Resistance
General Chemical Resistance
Certifications
Food contact, Food approval FDA 21 CFR
Applications
Medical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.